Die Head Acceptance and First-Week Faults

How a die head is accepted: the free test on your own material, the readings to demand, the handover report, and the faults that show up in the first week.

A die head is accepted with the line, not separately: a free test on 10–20 kg of the buyer’s material with video, measured output, specific energy and pellet photos before the balance is paid, and a deposit that is refundable if the measured output misses the agreed figure by more than 5%.

What the buyer should demand on the die itself is narrow and specific: a face held to plus or minus 1 °C across its width under full load, a body rated for the pressure the screw makes, and strands of even thickness across the face. Anything less is a die that will be argued about in month two.

Accept the die, not the bag

  • Ask for strand and die-face photographs, not only pellets, before the balance is paid.
  • The face reading is taken under load: plus or minus 1 °C across the width.
  • Uneven strands in week one are a manifold or face temperature problem, not a cutter fault.
  • Fines of 0.5% are normal; 2% tells you to look at the blade and the strand.
Product render of TENGLONG recycling equipment isolated on white, paired with the discussion of die head acceptance and the faults that follow.
Product render of TENGLONG recycling equipment isolated on white, paired with the discussion of die head acceptance and the faults that follow.. Used here as a visual reference for die head acceptance and the faults that follow. Rendering, not a photograph of a customer plant.

Acceptance Is a Test With Written Conditions

Acceptance for a die head is part of the acceptance for the line, and the published terms are clear: a free test on 10–20 kg of the buyer’s material, with video, measured output, specific energy and pellet photos sent before the balance is paid. A run that falls short of the agreed output by more than 5% leaves the deposit refundable.

For the die specifically, the test has to show the strand or the cut face, not only the pellets in a bag. Output and specific energy prove the machine; a photograph of the strand at the trough, or of the die face, proves the die. Both are worth asking for before the balance goes out.

The test hall has material storage, water and a 500 kVA supply, with three simultaneous material runs, so comparing two suppliers on your own material is a practical exercise. Payment is 30% T/T deposit, 70% before shipment; L/C at sight above US$50,000, which tells you how the supplier is financing the machine.

What to Read on the Die at Handover

Rendered exhibition scene showing TENGLONG plastic granulation equipment on display, shown as trade-show context for die head acceptance and the faults that follow.
Rendered exhibition scene showing TENGLONG plastic granulation equipment on display, shown as trade-show context for die head acceptance and the faults that follow.. Shown here as production context. Rendering, not a photograph of a customer plant.

The die face should hold plus or minus 1 °C across the face under full operating load, and that reading is taken under load rather than during warm-up. A die that has never been run at temperature will read well on its own heaters and badly in service, which is why the check belongs to the acceptance test and not to the delivery.

The pressure rating is the other reading. Screw pressure sets the ceiling: a twin screw extruder works at 200–300 bar and some high-torque lines exceed 400 bar, so a die body not built for it bulges and loses dimensional accuracy. Ask for the rating in writing, and ask to see a die that has been through a run.

Then look at the strands themselves. Equal thickness across the face means the manifold is doing its job; one thick strand and several thin ones means it is not. On a water ring pelletizer the die face is also the cut surface, so the same check can be made on the cut slug.

Commissioning and the Paperwork

On site, commissioning takes 7–10 days for a line and 3–5 days for a single machine, including commissioning, two days of operator training and a signed handover report. The handover report is the document that matters: it is where the die configuration, the measured output and the agreed tolerance are written down for both sides. On a turnkey plant the same document has to cover the wash side as well, so the die figures are signed off against a process, not against a bag of pellets.

Startup is 25–40 minutes from cold and 10 minutes from a 120 °C standby. The die is the last part of the machine to come up to temperature and the first part to be judged, so a plant that forms an opinion on strand quality in the first ten minutes is judging a die that has not reached temperature yet.

Warranty runs 18 months from commissioning or 24 months from shipment, whichever comes first, and wear parts are stocked for three years. A spare die plate sits inside both of those commitments: it is a wear part, and it is the item most often left off the packing list.

The Faults That Appear in the First Week

Uneven strands are the first fault, and they are nearly always a manifold or a temperature problem. Every hole needs the same pressure and the same temperature to feed it, and a die that does not manage that produces strands of different thicknesses, which the cutter then turns into pellets of different sizes. Nothing in the drive or in the screw will fix that.

The second fault is a size spread that appears only when output goes up. Push the line to its rated output and the pressure drop across the land changes; if the die was specified for half that output, the strands stretch and the pellet size follows them. Output is finished bagged pellets, averaged over four hours, so a die that only looks right at low rate passes a short trial and fails a week of production.

The third fault is heat. A long land gives a better melt strength and a more cylindrical strand, and the same extra heat it holds in the melt is what heat-sensitive grades cannot carry. If the first week shows yellowing, a smell in the pellets or a stickier cut than expected, the land ratio is the first thing to question, not the blade.

Fines, Dust and What Counts as Normal

A fines level of 0.5% is the normal condition and 2% is a maintenance signal. That figure comes from the blade side more often than from the die side, because blade condition sets dust level, but a die that produces ragged strands will raise the fines figure even with a sharp blade.

Spare parts are the practical answer to most first-week complaints. The standard spares package consists of a spare screw, a die plate and two screen packs, a combination that holds unplanned stops below 2%, with wear parts stocked for three years. If the handover report does not list the fitted die plate, its hole configuration and its diameter, you cannot order a matching replacement and you will not know what you are running.

Ask for the die specification and the quality control record of the test run in the same email, and check the figures against the platform you have bought from the comparison of 12 models. Then read the applications page to confirm that the grade in the specification is one the platform was built for, and if you want to see a die made rather than a photograph of one, the factory is 2.5 hours by high-speed train from Jinan and 1.5 hours by air from Shanghai, and a typical visit takes half a day.

First-week faults and where to look for them

The table sets out first-week faults and where to look for them. Treat it as the sheet you fill in before the supplier leaves the plant.

Symptom Most likely cause Where to look first
Strands of unequal thickness across the face Manifold not distributing melt evenly Hole pattern and manifold channels
Size spread appears only at rated output Die specified below the line output Land length and pressure drop
Yellowing or a smell in the pellets Excess residence time in a long land Land ratio against the grade
Fines above the normal 0.5% Blade condition, or strands that are ragged Blade edge and strand surface
Face temperature varying edge to edge Too few heater zones on a wide die Zone layout and sensor positions
Machine stalls when output is pushed Die body not rated for the screw pressure Body rating against 200–300 bar

Frequently asked questions

Q1: How is a die head accepted before payment?

A free test runs on 10–20 kg of the buyer’s material, and video, measured output, specific energy and pellet photos are sent before the balance is paid. If the measured output misses the agreed figure by more than 5%, the deposit is refundable.

Q2: What should the die face temperature be at handover?

The die face should hold plus or minus 1 °C across the face under full operating load. That reading has to be taken while the machine is running at rate, because a die that has only been heated on its own heaters will look correct and behave badly.

Q3: What is the most common first-week die fault?

Uneven strands across the face, caused by the manifold or by uneven face temperature. A coat-hanger or T-type manifold gives every hole the same pressure and temperature, and a die without one produces strands the cutter turns into uneven pellets.

Q4: How much fines are acceptable?

A fines level of 0.5% is normal running, and 2% is where a maintenance signal appears. Blade condition sets dust level, so a rising fines figure points at the cutter first, but ragged strands coming from the die will push the same figure up with a perfectly sharp blade.

Read next, if the same model is going on your line: Die Head: What It Contains and How It Shapes the Melt, Die Head Hole Size and Land Length: What Sets the Pellet, Sizing a Die Head and What It Costs and Choose a Die Head by Starting With the Pellet You Need.

About the author

Zhou Gong (周工) is a recycling machinery engineer at TENGLONG Plastic Machinery in Linyi, Shandong, where 30-plus staff work across 18,000 m² and 12 machine platforms covering 100 to 3,000 kg/h. I look at the strand before I look at the pellets, because the strand shows the fault days before the pellet sample does. Every figure used here has been measured on a machine or taken from a dated published source, not from a brochure.

Send the material form, the contamination level and your target output to our engineering team and you get a model and a price range within one working day. A test run on 10-20 kg of your own material is free, and if the measured output misses the agreed figure by more than 5%, the deposit is refundable.