Summary: Single screw granulation is a chain of physical changes, and every fault in the finished pellets was created somewhere upstream of the cutter. This article walks the material through that chain in four functional zones and states what changes at each one: solids dragged forward into a bed, compressed and melted across six PID zones at 190 to 240 °C, vented of moisture and ink volatiles through three venting stages, filtered through a double-piston hydraulic screen changer with 40 to 80 mesh packs, then shaped into strands, quenched in a 4 m water bath, cut by a 12-blade cutter at 300 to 900 rpm and classified on a vibrating screen. The closing section explains why a single screw is the most form-sensitive of the granulators: its output follows the bulk density and the shape of the feed before any setting is touched.

One pass through the barrel, start to finish
Material enters through a force feeder or a gravity hopper, passes a metal detector, and is drawn forward by a rotating screw in a 30:1 barrel. It is compacted into a solid bed, melted across six PID zones between 190 and 240 °C, vented of moisture and ink volatiles through three venting stages, filtered through a double-piston screen changer with 40 to 80 mesh packs, pushed through a die into strands, quenched in a 4 m water bath, dried by an air knife, cut by a 12-blade cutter at 300 to 900 rpm, and classified on a vibrating screen before the pellets reach a 25 kg bag or a silo.
Two published alternatives sit at the end of that line. A die-face water ring cutter can replace the strand bath, and the strand bath is the reference route for the reference pellets — see the TL-ST strand pelletizing line and water ring versus strand versus underwater. Which fits depends on floor space and on the pellet shape your customer buys, not on the extruder.
Why the four zones are the right division
Cutting the machine into zones rather than into parts keeps the diagnosis physical. Every downstream fault originates in the zone before it, so naming the zones in material order is also the order in which faults are read.
Zone one: solids transport, where a single screw has no second chance
A single screw conveys solids by drag. The flight walls rub against the material, and the material moves because the channel is filling and the screw is pushing it forward. That mechanism has one condition attached: the feed must be continuous and reasonably dense, or the channel stops filling and the screw runs partly empty.
Which is why output on a single screw follows the feed before it follows the drive. The published bands are quoted on LDPE film at 85% bulk density with 3% moisture, and the page states the two directions that effect takes: HDPE bottle flake runs 15 to 20% higher because its bulk density is better, while high-ink film runs about 10% lower because the screen pack must be finer. A feed that arrives in surges does not average out; the screw takes the surges.
Two published conditions belong to this zone rather than to the machine. Feed must be smaller than 30 mm and free of sand, metal and paper, and the material enters through a force feeder or a gravity hopper with a metal detector protecting the screw. Where the feed is film or light fibre, the answer is upstream: a compactor or agglomerator that densifies it before it reaches the screw, in the TL-FL film granulating line configuration.
Zone two: compression, melting and venting
Once the bed is established, the screw does three things at once: it compresses the material against its own path, generates shear, and moves the melt forward. The compression ratio — feed channel depth over melt channel depth — sets how hard that happens, and it is the figure the sheet does not print. L/D is printed instead, at 30:1 with 28:1 to 33:1 optional, which tells you how much barrel length exists for feeding, venting and melting to share.
Heat arrives in two ways. The barrel heaters deliver it, and the shear in the compressed material generates some of it. Heaters are published as PID control in six zones at ±1 °C with melt-pressure and melt-temperature alarms, and the process description puts the polymer at 190 to 240 °C across those zones. The ±1 °C is how tightly a zone holds its set point.
The barrel carries three venting stages, and the process description names two vacuum vents whose work is to pull moisture and ink volatiles out before they reach the melt. That is the mechanism behind the published statement that washed flakes with up to 3% surface moisture still produce a stable strand, and it is why polyolefins need no pre-drying step.
Where residence time is spent
Length is a budget, and the 30:1 barrel spends it in a fixed order: feeding, then venting, then melting, then the pressure-building section before the screen changer. Shortening the barrel also removes vent positions, which is why the optional 28:1 and 33:1 ratios are quoted with the material in mind.
Zone three: filtration, where the pressure is set
Filtration is published as a hydraulic double-piston screen changer with 40 to 80 mesh packs, and the geometry is deliberate: one cavity works while the other is exchanged, so a screen change does not interrupt output. The pack holds back paper, sand and unmelted specks, and the pressure it creates is what the melt sees on the way to the die.
That makes the screen a process instrument, not a filter. A rising pressure trend between changes is the earliest signal that the feed has changed, and it arrives before the pellets do. Where output stability matters more than screen life, the published melt pump option holds output to ±0.5% and takes the pressure dip out of a screen change.
Screen life is therefore an output number in disguise. Every hour lost to a blocked pack is an hour of melt pressure rising and output falling, and the test protocol logs the screen pack alongside output, melt pressure, melt temperature and kWh on every four-hour factory run — see how every line is factory tested.
Why the double-piston geometry matters commercially
An interrupted screen change is lost output, and lost output is paid for twice because the labour is already on shift. A changer that keeps one cavity working turns a routine stop into scheduled work with no production penalty.
Zone four: strand, quench, cut and classify
Melt leaving the die is shaped into strands by the die face, and the strand carries the pellet geometry. The published route is a 4 m water bath, an air knife to dry the surface, and a 12-blade cutter at 300 to 900 rpm to cut the cooled strand into pellets of 2 to 4 mm with a tolerance of ±0.2 mm. The air knife matters more than its size suggests: surface water on a pellet shows up later as a fused pellet in the bag.
Cutting is a matching job between three numbers: strand diameter, cutter speed and blade condition. Run the cutter above the match for a thin, stiff strand and the cut becomes a tear, which produces fines and length variation. A worn blade shears well on one side and tears on the other, and the defect clusters in one quadrant of the strand.
Finally the vibrating screen removes fines and longs, the last quality gate before the 25 kg bag or the silo. The alternative end of this zone is die-face cutting: the published water ring option replaces the bath and the strand, saves floor space, and produces a rounder pellet with a dewatering step attached.
Why the single screw is the most form-sensitive of the granulators
Compare the two ways a screw can move material. A single screw drags it, and drag conveying depends on the material filling the channel. A twin screw, with intermeshing flights, separates and conveys at the same time, and its conveying depends on screw geometry rather than on the state of the feed. That difference is why feed form decides so much on a single screw line.
Four consequences follow, and all four show up as output problems rather than machine faults. Low bulk density starves the channel, so film needs densifying first. A rigid regrind with paper and label fragments carries contamination that a 40 to 80 mesh pack will always catch, so washing comes before granulating. A feed that arrives in surges produces output that surges. And a screw profile cut for one polymer family will not melt another, which is why compression ratio matters more here than on a machine whose conveying does not depend on the feed.
The practical consequence is a rule: on a single screw granulator, most throughput problems are feed problems, and the fix is upstream. That is why the machine is specified around what it can swallow rather than what it can melt — the published feed condition of material smaller than 30 mm, free of sand, metal and paper, is the real specification. The full data is on the TL-SJ single screw granulator page, and the selection logic by feed form on granulator types compared.
The exception worth knowing
A melt pump changes the arithmetic of this zone. Holding output to ±0.5% decouples the delivered rate from the pressure fluctuation of a screen change, making the granulator less sensitive to short-interval contamination. It is worth pricing wherever the feed is dirty.
| Stage | What physically changes | Published figure that governs it | Feed form that stresses it most |
|---|---|---|---|
| Feed and solids transport | Loose solids are dragged forward and compacted into a bed | Force feeder or gravity hopper, feed under 30 mm, metal detector | Light film at low bulk density, which starves the channel |
| Compression | Channel depth reduces, pressure and shear rise, solids become a dense bed | 30:1 L/D with 28:1 to 33:1 optional; compression ratio not published | Rigid regrind and lumps, which need more compression than film gives |
| Melting | Solid bed becomes a continuous melt, driven by heaters and shear | Six PID zones at ±1 °C, melt window 190 to 240 °C | Mixed polymers, whose melting points sit 10 to 15 °C apart |
| Venting | Moisture and ink volatiles are pulled out of the melt | Three venting stages, two vacuum vents; 3% moisture reference | Printed and washed film, the highest gas load in the range |
| Filtration | Paper, sand and unmelted specks are held back; melt pressure is set | Double-piston hydraulic changer, 40 to 80 mesh, no output interruption | Unwashed post-consumer feed, which sets the screen interval |
| Strand, bath and cut | Melt becomes strands, the skin freezes, the strand is cut into pellets | 4 m bath, air knife, 12-blade cutter at 300 to 900 rpm, 2 to 4 mm ±0.2 mm | Stiff or filled grades, which tear instead of shearing when cut |
Frequently asked questions
Q1: What happens inside the barrel of a single screw granulator?
Four things happen at once, which is why a single screw is sensitive to feed shape. The screw compacts the material against its own path, generates shear, melts it against the barrel heaters, and vents moisture and ink volatiles through three venting stages. The barrel is 30:1 L/D with 28:1 to 33:1 optional, heated in six PID zones at ±1 °C across a 190 to 240 °C melt window.
Q2: Why does a single screw granulator starve on mixed film and rigid regrind?
Because a single screw conveys by drag, and drag conveying needs the channel to stay full. Light film at low bulk density leaves gaps, and the screw runs partly empty, so output falls and pulses. The published reference is LDPE film at 85% bulk density, and HDPE bottle flake runs 15 to 20% higher for exactly this reason. Film needs densifying upstream.
Q3: What do the venting stages in the barrel of a single screw actually remove?
Two things: water vapour and volatiles from printing inks. The published barrel carries three venting stages, and the process description names two vacuum vents doing that work, which is what allows washed flakes with up to 3% surface moisture to produce a stable strand without pre-drying. A blocked vent changes the melt temperature with no change in the barrel setting.
Q4: How does the double-piston screen changer hold output steady during a screen change?
Because it works on two cavities. One cavity is filtering while the other is being exchanged, so the changeover happens in parallel with production and output does not drop. The published specification is a hydraulic changer with 40 to 80 mesh packs. The trade-off is pressure: the pack sets the back pressure the melt sees, so the mesh fit sets your screen interval, and with it your real output.
Q5: How does the strand reach a 25 kg bag, and where does the pellet size come from?
The die face shapes the melt into strands, a 4 m water bath freezes the strand skin, an air knife dries the surface, and a 12-blade cutter at 300 to 900 rpm cuts it into pellets of 2 to 4 mm with a tolerance of ±0.2 mm. A vibrating screen removes fines and longs before the pellets drop into a 25 kg bag or a silo.
Engineer’s note
When I walk a new plant through a TL-SJ, I spend most of the time on the first zone, because everything downstream is a consequence of what the screw was fed. Our screws are 38CrMoAlA, nitrided in-house to a 0.5–0.7 mm case at HV 900–1000 and straightened to 0.03 mm runout over the full length, and barrel, screw, gearbox and frame are aligned to 0.05 mm. A tight screw cannot rescue an unsteady feed, and no temperature setting can either.
Engineering note: the numbers on this page are our own published reference ranges for the machine family, not a specification guarantee for any individual unit. Final output, specific energy and pellet quality are set by the incoming material, its moisture and contamination level, and the screen pack fitted. We write the confirmed figures onto the quotation after a factory test run on your own material.
Who wrote this
Zhou Gong (周工) is a senior plastic machinery engineer at TENGLONG Plastic Machinery in Linyi, Shandong. The factory was registered as Linyi Hedong District Tenglong Plastic Machinery Factory on 7 June 2016 and grew out of a screw and barrel workshop, so his work is rooted in the parts that decide whether a granulator holds output: screw geometry, nitriding case depth, barrel alignment and melt filtration. He prepares the technical specification for customer quotations, reviews the four-hour factory test data before shipment, and runs commissioning support on site. Screws are nitrided in-house to a 0.5–0.7 mm case at HV 900–1000 and straightened to 0.03 mm runout over the full length; barrel, screw, gearbox and frame are aligned to 0.05 mm before the test run.
Figures quoted here are engineering reference ranges published on our own product pages, not guaranteed values for any specific machine. Real output, specific energy and pellet quality depend on the incoming material, its moisture and contamination level, and the screen pack fitted. Final values are written after a factory test run on the customer’s own material, and the PLC-logged test report ships with the machine. For a quotation that reflects your material, send the feed form, contamination level and target output and a configuration comes back within one working day.
Send the polymer, the feed form, the moisture and the contamination level, and we will map the process stages onto your material and confirm the settings on a factory test run. Request the process map for your material — a reply comes back within one working day.