Summary: Single screw granulator faults are diagnosed wrong when they are diagnosed by guessing. This playbook starts from the data instead of the symptom. Every case follows the same sequence: the signal on the screen, what that signature means, the ranked causes behind it, and the first check that settles it. Seven common faults are covered — hopper bridging and feed starvation, melt temperature drifting high or low, polymer building up on the die face, the screen pack blocking every hour, uneven pellets, bubbles and voids in cut pellets, and the noise that means either a screw wearing or a bearing failing. The published figures are used throughout: 190 to 240 °C melt window, 40 to 80 mesh packs, a 12-blade cutter at 300 to 900 rpm, feed under 30 mm, and the 0.28 to 0.42 kWh/kg band.

Triage by the four numbers on the screen
Before anyone touches a set point, read four traces from the previous shift: melt pressure, melt temperature, kWh per kilogram, and the time since the last screen change. Those four tell you which part of the machine is arguing, and the order of the diagnosis follows the material: feed, then melt, then filtration, then the cut. On a single screw a feed problem becomes a melt problem, a melt problem becomes a pressure problem, and a pressure problem becomes a pellet problem — so treating the last symptom first costs a day of changing settings that were never wrong.
Two disciplines apply to every case here. Change one variable at a time and give the machine enough running time to settle before reading the result again. And write down what the data showed, because the PLC logs output, melt pressure, melt temperature and kWh every minute, and the same log on your shift turns an intermittent fault into a diagnosable one. The test protocol is on how every line is factory tested.
The order of the four checks
Feed, melt, filtration, cut. It looks obvious once written down, but it is the order most often reversed in practice, because the pellet is what the operator can see. On the TL-SJ single screw granulator the melt is prepared by a single screw with three venting stages, so a feed fault propagates through every stage below it.
The feed will not feed: bridging, starvation and surging
Signature in the data. Melt pressure falls away from the screen and kWh per kilogram drops, with no change in barrel temperature. Output either stops completely or arrives in bursts.
Why it happens. Light film flake at low bulk density forms a stable arch in the hopper, and a gravity hopper cannot break it. A force feeder solves this by design, which is why the published feeding options are a force feeder or a gravity hopper with a metal detector rather than an open chute. Two published feed conditions sit behind most of these cases: feed smaller than 30 mm, and free of sand, metal and paper. A bridged hopper is often a size-reduction problem upstream — see the crusher and shredder range — and a feed that varies in bulk density arrives at the screw as an output the machine cannot average away.
First checks. Confirm the feed actually reaching the barrel is under 30 mm and free of metal, then confirm the metal detector is live. Watch the hopper level: if material is bridging above the throat while the screw is running, change the feeding method before changing anything on the screw.
Melt temperature drifting high or low
Signature in the data. Melt temperature climbs over 10 to 20 minutes while kWh per kilogram falls, or melt temperature falls while kWh per kilogram rises. Both signatures point at the same place: the barrel.
Why it happens. Shear heating at high screw speed raises the melt temperature above the zone set points, and the PID controller then holds the zones correctly while the melt inside runs hot. The opposite case — melt temperature down, kWh up — is a heat input problem: zones set below the window for the polymer, or cold wet feed pulling the melt down. Both sit inside the published 190 to 240 °C melt window for the polyolefins this machine is sold for, and LDPE runs about 10 to 15 °C cooler than PP. A drifted sensor produces the high-temperature signature with no physical cause, which is why a hand-held probe check comes before any setting change.
First checks. Compare the PLC melt temperature with a probe on the melt itself. Then check the zone set points against the material you are actually running, and check the venting stages on the 30:1 barrel for a blockage, because a vent that cannot pull will let moisture and ink volatiles stay in the melt and change the melt temperature without any change in the barrel setting.
Polymer builds up on the die and the screen blocks every hour
Signature in the data. Melt pressure climbs in steps through the shift and drops back each time a pack is exchanged. Short intervals between screen changes are the symptom; the pack you pull out is the diagnosis.
Degraded skin, dirt, or the wrong mesh
Why it happens. Three causes, in the order they are worth checking. First, degraded polymer skin: material that has sat too long in the hot zone carbonises on the die face and comes off in flakes, and those flakes load the pack. Second, contamination that never belonged to the melt: paper, sand and metal fragments from an incompletely washed bale, and the screen is doing the job it was specified for. Third, a mesh finer than the dirt allows. The published range is 40 to 80 mesh, and the fine end on dirty feed guarantees short intervals; the washing line equipment route upstream is what actually changes the interval.
First checks. Open the screen changer and read what the pack collected — polymer dust means melt quality, foreign objects mean upstream control, and the two have completely different fixes. Check the die face for a skin. If the interval is the problem and the dirt is upstream, shorten the interval deliberately, fix the washing, and step the mesh one step coarser within the published range.
Uneven pellets, and bubbles inside them
Signature in the data. For uneven pellets: cutter speed drifting, strands of visibly different diameter leaving the die. For bubbles: nothing in the melt data, but the bulk density of the batch sits below what the customer ordered and pellets are hollow when cut open.
Why the size varies. The cutter is published as a 12-blade unit running at 300 to 900 rpm, matched to strand diameter. Run the cutter high against a thin, stiff strand and the cut becomes a tear instead of a shear, which generates fines and length variation. A worn or chipped blade shears well on one side and tears on the other. The published pellet specification is 2 to 4 mm with a tolerance of ±0.2 mm, so drift beyond that band is a fault.
Why bubbles appear. Moisture is the dominant cause and the one that actually creates voids: water in the flake vaporises inside the melt and the steam escapes through the cut face. The published output reference is quoted at 3% moisture, and above that level voids are close to guaranteed. Air entrained in a melt that is too cold or too fast produces the same result, and the two are told apart by distribution — air voids scatter, moisture voids cluster after a residence-time change. The pellets and feedstock glossary defines the contamination terms used here.
First checks. Measure moisture on the actual flake with a meter, not on a supplier data sheet. Reset cutter rpm in steps and watch one quadrant of the strand. Check blade condition and die face before reassembly.
Noise: a screw wearing through, or a bearing failing
Signature in the data. A low grinding note that rises with output, or a knocking sound whose pitch changes with screw speed. Melt pressure that trends upward at the same screw speed and the same feed.
Separating a wear item from a repair
Why it happens. Two quite different causes, worth separating early because one is a wear item and the other a repair. A worn screw or a scored barrel changes the flow geometry: material no longer fills the channel, the screw runs partly empty, and the pressure needed to push the same output rises. A bearing failure announces itself through vibration and heat at the drive end rather than through the melt. A third possibility is foreign material already in the machine, which is why the metal detector matters: a fragment that got past it damages the screw in a way no alignment will fix.
First checks. Pull the screen pack and look for metal. Check the screw and barrel for scoring and for the case depth on the flight lands, against the 38CrMoAlA nitrided specification of 0.5 to 0.7 mm at HV 900 to 1000. Check drive-end vibration and bearing temperature. Before blaming the screw for everything, confirm the alignment figures: barrel, screw, gearbox and frame are held to 0.05 mm on our lines, and a line re-set after a motor swap should be re-aligned before the screw is condemned.
| Symptom | Signature in the PLC data | Ranked causes | First check |
|---|---|---|---|
| Feed stops or arrives in bursts | Melt pressure and kWh fall away with no temperature change | Hopper bridging on light film, feed over 30 mm, metal in the feed | Watch the hopper level with the screw running; confirm flake size and detector |
| Melt temperature drifts up | Temperature rises 10 to 20 min, kWh per kg falls | Shear heating at high screw speed, thermocouple drift, a blocked vent | Probe the melt and compare with the PLC reading |
| Melt temperature drifts down | Temperature falls, kWh per kg rises | Zone set points below the polymer window, cold or wet feed | Check zone set points against the 190 to 240 °C window and the feed condition |
| Polymer builds up on the die face | Pressure climbs in steps, resetting at each screen change | Degraded skin from long residence, contamination, mesh too fine for the dirt | Open the pack and read what it collected; inspect the die face |
| Screen blocks every hour | Short intervals between pack changes, rising pressure between them | Paper, sand or metal upstream, 80 mesh run on dirty feed | Read the extracted pack; step the mesh coarser within 40 to 80 mesh |
| Pellets uneven or off the 2 to 4 mm band | Cutter speed drifting, strands of different diameter | Cutter rpm mismatched to strand diameter, worn blades, blocked die holes | Reset cutter rpm within 300 to 900 rpm and check blades and die face |
| Bubbles and voids in cut pellets | Melt data normal, bulk density below the ordered value | Moisture above the 3% basis, air entrained in a cold or fast melt | Measure moisture on the flake with a meter |
Frequently asked questions
Q1: Why does my single screw granulator keep blocking the screen pack every hour?
Read the pack you pull out. Polymer dust means the melt is degrading upstream and the die face is shedding skin; foreign objects mean sand, paper or metal is entering the melt and the washing route needs attention. The published filtration is a double-piston changer with 40 to 80 mesh packs, so the fine end of that range on dirty feed guarantees short intervals. Fix the cause first.
Q2: How do I stop light film flake from bridging in the hopper of a single screw?
Bridge a light, low-bulk-density feed is an arching problem, and the published answer is feeding: a force feeder or a gravity hopper with a metal detector, not an open chute. If bridging persists, check the feed itself — the published limit is material smaller than 30 mm, free of sand, metal and paper, and light film often needs densifying upstream. A variable bulk density also produces surging at the screw.
Q3: What causes unmelted specks and bubbles in the pellets from a single screw?
Unmelted specks point at heat input or feed size: zones set below the polymer’s window, a screw speed too high for the melting demand, or feed above the published 30 mm limit. Bubbles and voids are usually moisture: the output reference is quoted at 3% moisture, and above that, steam forms inside the melt and escapes through the cut face. Measure moisture with a meter.
Q4: How do I tell screw wear from a bearing failure on a single screw granulator?
Watch which number moves. Screw or barrel wear changes the flow geometry, so melt pressure climbs at the same screw speed and feed while the temperature stays normal. A bearing failure shows as vibration and rising temperature at the drive end instead. Metal already inside the machine is a third possibility, so check the extracted pack for metal first.
Q5: Why does the melt temperature change on a single screw after a screen change?
Two reasons. A screen change alters the back pressure at the die, and the melt temperature and pressure move with it until the melt re-equilibrates, so give the machine time before judging the new reading. A blocked vent is the second: the barrel carries three venting stages to pull moisture and ink volatiles, and a vent that cannot pull changes the melt with no change in the barrel setting.
Engineer’s note
Before I answer a fault on the phone I ask for two numbers: the melt pressure at the screen and the time since the last screen change. Together they tell me whether the line is starving, filtering or melting, and that saves a site visit. The reason I trust the trace is the test protocol: every machine runs four hours on the customer’s own material with output, melt pressure and kWh logged every minute, and that log ships as the commissioning baseline.
Engineering note: the numbers on this page are our own published reference ranges for the machine family, not a specification guarantee for any individual unit. Final output, specific energy and pellet quality are set by the incoming material, its moisture and contamination level, and the screen pack fitted. We write the confirmed figures onto the quotation after a factory test run on your own material.
Who wrote this
Zhou Gong (周工) is a senior plastic machinery engineer at TENGLONG Plastic Machinery in Linyi, Shandong. The factory was registered as Linyi Hedong District Tenglong Plastic Machinery Factory on 7 June 2016 and grew out of a screw and barrel workshop, so his work is rooted in the parts that decide whether a granulator holds output: screw geometry, nitriding case depth, barrel alignment and melt filtration. He prepares the technical specification for customer quotations, reviews the four-hour factory test data before shipment, and runs commissioning support on site. Screws are nitrided in-house to a 0.5–0.7 mm case at HV 900–1000 and straightened to 0.03 mm runout over the full length; barrel, screw, gearbox and frame are aligned to 0.05 mm before the test run.
Figures quoted here are engineering reference ranges published on our own product pages, not guaranteed values for any specific machine. Real output, specific energy and pellet quality depend on the incoming material, its moisture and contamination level, and the screen pack fitted. Final values are written after a factory test run on the customer’s own material, and the PLC-logged test report ships with the machine. For a quotation that reflects your material, send the feed form, contamination level and target output and a configuration comes back within one working day.
If a fault is not on this page, send the material, the symptom and the PLC trace from the shift, and we will narrow it from the same numbers we logged on our own test runs. Send the material and the PLC trace — a reply comes back within one working day.